manufacturer 24mm AR Chopped Strands in Bolivia. for the glass fiber reinforced cement and develop, generally USES the dry mixing or wet mixing process, add the amount in 1-5%, 50 RPM speed, the mixing time for 20 minutes. Mixed with cement mortar and other materials, it has a good cluster. It is not divided into monofilament, with "Y" type on both ends, which enhances the grip of cement.